you will see where he says he anneals these pieces from 1 to 2 1/2 weeks, is this for real? what do you folks think, what would be a good and proper annealing schedule for things like this
thanks
rodney
IS THIS FOR REAL,,,,,,ANNEALING
Moderator: Brad Walker
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Yes, it's for real. It's not unusual for thick pieces to require days (even weeks) of annealing time.
Bullseye has some information on annealing for thick pieces on their website: http://www.bullseyeconnection.com/pdfs/ ... _thick.pdf
Bullseye has some information on annealing for thick pieces on their website: http://www.bullseyeconnection.com/pdfs/ ... _thick.pdf
I was there visiting
and the work is awesome. I even bought a blown vase there the prices were very reasonable.....I saw those pieces and they are very thick and beautiful. When I was down in Florida at a blown glass place they blew on Friday nite and then annealed until Sunday afternoon. (There pieces were not any where near the thickness of the ones on this page.) That was when you could come back and see the piece after it was finished annealing.
-
charlie holden
- Posts: 260
- Joined: Thu Mar 13, 2003 8:26 pm
- Location: Atlanta
I used to have a picture on my fridge of Charlie Miner's grand daughter INSIDE of of his big ones, about 4' across by 3' high. He built a special kiln just to cast these monsters, it's round, about 5' by 4'. All dimensions approximate. Brock
My memory is so good, I can't remember the last time I forgot something . . .
-
Rocky Gentry
- Posts: 14
- Joined: Sun Mar 09, 2003 3:40 pm
- Location: St. Petersburg, FL