Kiln furniture for small pattern bars?
Posted: Sun Dec 07, 2003 6:58 pm
I was wondering if it would be possible to use the hole in kiln furniture for small pattern bars and millefiori/murrini like stuff?
What I was thinking is to either kilnwash the inside and outside or line it with thin fire and fill with glass, stand on end and fire like that. Hopefully producing what I want, and not exploding the kiln furniture in the process.
Has anyone tried this? Is it do-able or are there foreseeable problems?
I have the murrini maker mold, but want something a little different.
What I was thinking is to either kilnwash the inside and outside or line it with thin fire and fill with glass, stand on end and fire like that. Hopefully producing what I want, and not exploding the kiln furniture in the process.
Has anyone tried this? Is it do-able or are there foreseeable problems?
I have the murrini maker mold, but want something a little different.