bowls are not shiny on their rims after I slump them..Help
Posted: Tue Dec 16, 2003 3:59 pm
by deborahbur
I have tried most everything. My round rice style bowls are fine on their edges when I fuse them but get cloudy when I slump them? Any ideas?\
Thanks
Deborah
Bowls are 7" across flat
Posted: Tue Dec 16, 2003 6:47 pm
by jerry flanary
Do you have this trouble w/ all color combos? Is it devit? Have you invested in a cold shop?
Posted: Tue Dec 16, 2003 9:13 pm
by Barbara Muth
is the first firing on thinfire?
Posted: Tue Dec 16, 2003 9:18 pm
by deborahbur
All colors are cloudy around the top.......yes the first firing was on thin fire.
What kind of cold work?
Thanks
Deborah