Page 1 of 1
Metallic Gold Paint
Posted: Sat Dec 20, 2003 8:56 am
by Greg Rawls
Does anyone know where to find metallic gold paint? I want to paint a rim on a bowl. I've seen the ink-type gold, but I'm looking for something more like paint. Thanks!
Greg
http://www.gregorieglass.com
Posted: Sat Dec 20, 2003 9:22 am
by Tony Smith
Greg,
Do you mean the Hanovia Bright Gold? It matures pretty low... at about 1100° and gives a solid, bright finish.
You should be able to find it from CRLoo, Ed Hoy or any ceramic supply house.
Tony
Posted: Sat Dec 20, 2003 10:11 am
by Bert Weiss
The bright gold lusters come in 2 temperatures, one for glass and one for ceramic. Besides Hannovia, Ferro makes it as well. This is the stuff used for the gold rims on Annie Glass.