luster disaster
Fused an 18 " diameter blank, 1/4 inch thick, clear BE with different colors strips of transp. and opaque....fused gr8......Then experimented with covering the surface with hanovia SP rainbow luster..to get a peralized look but all I got was peralized disaster.......fused up to 1300 per instructions.....What is the best way to get it off.....Didnt really want to sandblast because I wanted a shiny finish? Can this be restored?
Also, having a problem with my kiln wash BE on shelf....Chipping off after only one firing and I use thin fiber paper? Is wash too thin...too thick...or what? That was my surprise for x-mas.....
Also, having a problem with my kiln wash BE on shelf....Chipping off after only one firing and I use thin fiber paper? Is wash too thin...too thick...or what? That was my surprise for x-mas.....
-
Geri Comstock
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: luster disaster
Docdoctac wrote:Fused an 18 " diameter blank, 1/4 inch thick, clear BE with different colors strips of transp. and opaque....fused gr8......Then experimented with covering the surface with hanovia SP rainbow luster..to get a peralized look but all I got was peralized disaster.......fused up to 1300 per instructions.....What is the best way to get it off.....Didnt really want to sandblast because I wanted a shiny finish? Can this be restored?
Also, having a problem with my kiln wash BE on shelf....Chipping off after only one firing and I use thin fiber paper? Is wash too thin...too thick...or what? That was my surprise for x-mas.....
You can sandblast and fire polish. It will come right back to shiny. Tony Smith knows what temps. I don't.
What was the look you got? was it overfired? was it applied too unevenly?
I will guess that your wash it too thick. I use an extremely thin wash when firing float glass and it never chips. My wash is the consistency of skim milk. I'll bet your using heavy cream. Try thinning it down and applying more coats.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact: