I just purchased my first kiln about two weeks ago.  So far I am fusing small projets and scrap glass to get a "feel" of the kiln.  I have a question about using glue to hold glass in place.  I made a small coaster project, and I glued the top piece to the bottom piece to keep the overhang consistant.  the final product looks like there are bubbles where the glue may have been.  I used "Welbond" glue, would that cause a problem
Garry
			
			
									
						
										
						Fusing & Glue
Moderators: Brad Walker, Tony Smith
Re: Fusing & Glue
hi gary - alot of people use elmer's glue - just a very SMALL dab - you can use either the original white glue or the new blue gel - my personal perference is the gel - dries clear and i haven't had problems if i take a couple of days to work on a shelf full of things, but remember you only need a VERY SMALL dabvanpool wrote:I just purchased my first kiln about two weeks ago. So far I am fusing small projets and scrap glass to get a "feel" of the kiln. I have a question about using glue to hold glass in place. I made a small coaster project, and I glued the top piece to the bottom piece to keep the overhang consistant. the final product looks like there are bubbles where the glue may have been. I used "Welbond" glue, would that cause a problem
Garry
D
I find the key to successfully glueing projects is not so much which glue you use, but WHERE you put it.  I use a tiny dab, on a toothpick, and put it as close to the edge of the glass that is being glued as possible.  This prevents bubbles and residue being trapped under the glass after firing.
JoanB
			
			
									
						
										
						JoanB
- 
				Judy Schnabel
 - Posts: 195
 - Joined: Mon Mar 10, 2003 9:45 pm
 - Location: SW FL
 - Contact:
 
- 
				LesleyNolan
 - Posts: 21
 - Joined: Fri Mar 14, 2003 5:17 pm
 - Location: Tallahassee FL
 - Contact:
 
I use elmers glue diluted with water 50/50.  As mentioned before, you do have to use just a tad.  If you use too much you can create carbon bubbles.  This is where as the glue burns off, the carbon residue is trapped in the glass.  The bubbles are black/silver.  
To prevent the bubbles use only the smallest amount to secure your pieces and hold in the 1100 - 1200 range for about 30 min to make sure that all the glue burns out before fuse. Also if you go slowly up in the first place it helps.
In my work with lots of little pieces I have to glue them. They are usually on top of the base glass which also prevents glue bubbles.
I have never used super glue but I know that elmers is cheaper!
Hope this helps,
Lesley
			
			
									
						
										
						To prevent the bubbles use only the smallest amount to secure your pieces and hold in the 1100 - 1200 range for about 30 min to make sure that all the glue burns out before fuse. Also if you go slowly up in the first place it helps.
In my work with lots of little pieces I have to glue them. They are usually on top of the base glass which also prevents glue bubbles.
I have never used super glue but I know that elmers is cheaper!
Hope this helps,
Lesley
- 
				ernest porcelli
 - Posts: 18
 - Joined: Tue Mar 11, 2003 6:41 pm
 - Location: Brooklyn, NY
 - Contact:
 
Glue?
i use elmer's for some projects, but what i found to work the best to get large pieces (25x25) into by kiln is scotch tape 3M majic tape.
tape the glass on the bottom ,use fiber paper, almost all my works have clear top glass,so i use it(top glass) to slide the taped glass into the kiln , like it was a pizza pie.this i've done for years. i've also used the tape between both layers, no problem,if you are taping both layers, card board will be used to slide the glass into the kiln, just don't use the tape on the top. good luck, by the way it helps to cut the top piece of glass 1/8 " bigger ep
			
			
									
						
							tape the glass on the bottom ,use fiber paper, almost all my works have clear top glass,so i use it(top glass) to slide the taped glass into the kiln , like it was a pizza pie.this i've done for years. i've also used the tape between both layers, no problem,if you are taping both layers, card board will be used to slide the glass into the kiln, just don't use the tape on the top. good luck, by the way it helps to cut the top piece of glass 1/8 " bigger ep
-EP