Page 1 of 1
Copper Wire fused between glass
Posted: Mon Jan 05, 2004 10:09 pm
by bheath
Can anyone help me with the name of a product or a procedure that protects the color of copper wire fused in between two pieces of glass and fired at full fuse?
Posted: Mon Jan 05, 2004 10:22 pm
by Mira
I think I read in the archives that a borax solution will do it. Sorry, don't know the exact formula, though.
Mira
Posted: Tue Jan 06, 2004 1:36 am
by Lyn
Mine turned redish I was just wondering what color background glass would go well with it. Do you use the borax between layers of glass? I've just heard of it used on the surface. My sterling wire has a light yellow around it, is the fix for that using fine silver? Lyn
http://community.webshots.com/user/lynfeu
Posted: Tue Jan 06, 2004 7:31 am
by Tony Smith
Lyn wrote:Mine turned redish I was just wondering what color background glass would go well with it. Do you use the borax between layers of glass? I've just heard of it used on the surface. My sterling wire has a light yellow around it, is the fix for that using fine silver? Lynhttp://community.webshots.com/user/lynfeu
The yellow around your silver wire is called silver stain. It is caused by silver leaching into the glass. If you use silver, there's a chance you'll get silver stain. Like the irid problems in another current thread, it's not always consistent.
Try using nichrome wire instead. It stays bright and shiny and is much stonger than silver when you form your loops. You can get various diameters and lengths from McMaster-Carr at
http://www.mcmaster.com page 3398 in their current online catalog. They call it nickel chromium wire or Chromel C.
Tony
Posted: Tue Jan 06, 2004 7:54 am
by Lyn
Thanks Tony, I did get some nicrome wire and it stays nice as a loop for a chain. Haven't tried it between layers of glass. The silver stain looked like frost on branches thought I might use it that way.
Posted: Tue Jan 06, 2004 7:55 am
by Tom White
I have kept sheet copper inclusions bright by coating them with clear Unique Glass Paint before fusing. I get some bubbles on the copper. You can see at
http://photos.yahoo.com/tomwhite2
Best wishes,
Tom in Texas
Posted: Tue Jan 06, 2004 11:28 am
by Lyn
Very graphic example on the 2nd star. Thanks. I've also wondered about watercolor lusters, tried sharpies in gold and silver after someone said they worked on glass, the silver worked well gold didn't for me.
Thanks to all,
this forum is a wonderful source
Lyn
Posted: Tue Jan 06, 2004 12:06 pm
by bheath
Thanks for all your helpful suggestions. This is my first time on and I agree with Lyn, this forum is a wonderful source

Posted: Tue Jan 06, 2004 1:45 pm
by Judy Schnabel
Tom,
How do you apply the clear Unique?
I took your suggestion first time I tried firing the copper between two layers of float. But I used a little sponge brush and the brush marks showed after it was fired. Do you use an airbrush?
Also, what gauge copper are you using? I just received the sample from Nimrod Hall.
Has anyone used pearl-ex on copper then firing it?
Judy
Posted: Wed Jan 07, 2004 12:35 pm
by Wayne
Where do you get clear unique

Posted: Wed Jan 07, 2004 1:34 pm
by Judy Schnabel
I'm not at my own computer right now but I believe you can find Unique Paints at
http://www.crestmolds.com
Judy