I did a course about 2 years back and we used a white powder around the edge of our slump designs for float.
Does anyone know what that white powder could have been or perhaps what i could use to give an uneven look to the edges of float plates?
Cathy
Does anyone know what that white powder could have been or perhaps what i could use to give an uneven look to the edges of float plates?
Cathy
Cathy
http://www.chockadoo.com
http://www.chockadoo.com
-
Linda Denli
- Posts: 21
- Joined: Wed Aug 27, 2003 2:58 pm
- Location: London, UK
Hi Cathy, I think you might mean Effotobolle powder which is available in lots of colours and creates a blistered bubble effect when it is sandwiched between two sheets of glass. the supplier says it is compatible with all kinds of glass but I have only tried it with clear Spectrum 96 brought up to full fuse temperature. Results are a bit hit and miss, sometimes it bubbles and sometimes it doesn't and sometimes you get lots of little bubbles and one huge one, but it is quite fun. You could also try sprinkling some bicarbonate of soda/baking powder between the layers of glass as this gives a similar effect.
Regards
Linda
Regards
Linda
Linda from London
-
Kathie Karancz
- Posts: 137
- Joined: Wed Mar 12, 2003 3:49 pm
- Location: Calgary, Alberta, Canada
- Contact:
-
Kathie Karancz
- Posts: 137
- Joined: Wed Mar 12, 2003 3:49 pm
- Location: Calgary, Alberta, Canada
- Contact:
Signature bowl
Hi Kathie,
I've fused lots of iridised pieces with dichroic, clear, and may colours so far without any problems. The Sun is the sunflower yellow bullseye colour. Only thing I would change is I would put a layer of clear between the iridised and the sun. I love the glossy effect of glass so wasn't as keen on the matted iridised feel. Its contrasting in texture which I guess makes it more interesting.
The only colours I have so far had problems with are the white and madri gra cranberry and clear. Out of 5 pieces 2 cracked badly and recracked after refusing. DOH!
Cathy
I've fused lots of iridised pieces with dichroic, clear, and may colours so far without any problems. The Sun is the sunflower yellow bullseye colour. Only thing I would change is I would put a layer of clear between the iridised and the sun. I love the glossy effect of glass so wasn't as keen on the matted iridised feel. Its contrasting in texture which I guess makes it more interesting.
The only colours I have so far had problems with are the white and madri gra cranberry and clear. Out of 5 pieces 2 cracked badly and recracked after refusing. DOH!
Cathy
Cathy
http://www.chockadoo.com
http://www.chockadoo.com
-
Linda Denli
- Posts: 21
- Joined: Wed Aug 27, 2003 2:58 pm
- Location: London, UK
I got my Efotobolle powder from a supplier called Creative Glass and you can find them on http://www.creative-glass.com.
They have studios in the UK and Switzerland, but I'm not sure if they have a set-up in the US.
I haven't done it yet but I thought I'd try mixing some baking powder and coloured glass enamel together- just to see what happens - has anyone tried this??
Best wishes
Linda
They have studios in the UK and Switzerland, but I'm not sure if they have a set-up in the US.
I haven't done it yet but I thought I'd try mixing some baking powder and coloured glass enamel together- just to see what happens - has anyone tried this??
Best wishes
Linda
Linda from London
Hi Linda,
My partner and I were thinking of trying the baking soda tomorrow so I'll let you know how it goes.
Kind regards
Cathy
My partner and I were thinking of trying the baking soda tomorrow so I'll let you know how it goes.
Kind regards
Cathy
Cathy
http://www.chockadoo.com
http://www.chockadoo.com
I haven't tried baking soda and glass enamels with fusing yet, but with a torch the enamels get all bubbly and crusty. Kind of ancient looking. Bead artists have commented though that their baking soda beads seem really unstable and many crack. So maybe the baking soda needs to be "neutralized" at some point in the process.