Page 1 of 1
boron nitride
Posted: Tue Jun 26, 2012 6:48 pm
by Karyn Cott
I have a can of boron nitride and was wondering if you all like to use it on stainless steel or do you feel that kiln wash works better?
Re: boron nitride
Posted: Tue Jun 26, 2012 7:01 pm
by Brock
A properly prepared SS mold can last YEARS with KW . . .
Re: boron nitride
Posted: Tue Jun 26, 2012 7:27 pm
by Karyn Cott
One other question. I am draping over a ss form for a lamp shade. I want somewhat of a texture to the inside so that the light from the bulb is diffused. Would it work if I draped fiber blanket (that I separate into a thinner piece) over the ss form?
Re: boron nitride
Posted: Tue Jun 26, 2012 8:48 pm
by Brock
It would be better to impart the texture to the shade in a hotter firing on a kiln shelf. Then slump.