fusing 96 white streaky to clear
Posted: Mon Jul 23, 2012 12:28 pm
I have a piece of 96 about 8"x10" that I want to fuse to a piece of clear 96. Normally I would go about 350 degrees to 1000, hold 8, then 350 to 1225, hold 15, then 500 to 1350, hold 45. Due to its size, I'm wondering if this is sufficient time at the holds to make sure I get a good smooth piece, with no blow-outs. I fuse on the kiln shelf, with no shelf paper.