Post by wingoda »

I thought that it would be fun to take a blue bottle and recycle it into a moble. So I smashed it into course chuncks and places it in a clay mold. I fired it several times hoping it would melt/fuse but I have been stumped so far on how hot it needs to go. The last attempt was 1800 degrees with a 10 minute hold and the chuncks were rounded a bit but did not even tack fuse together. They were loosely joined in the mold but when I picked them up all the chuncks fell apart... Does anyone have a general idea of the right temperature range? Also the pieces appear to have a great deal of divit on them from mutliple firings.

Regards,
David
David Wingo
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Blue bottle glass - melting temp?

Post by Kevin Midgley »

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Blue bottle glass - melting temp?

Post by rosanna gusler »

throw them away and start over. once they devit like that they do not want to melt or stick. i do not fire blue glass bottled higher than 1515f. rosanna