Page 1 of 1
Almost There
Posted: Fri Sep 07, 2012 1:58 pm
by Yardic Glassworks
I've been playing around a bit with getting some multi-colored castings. This was the first practice model.
Re: Almost There
Posted: Fri Sep 07, 2012 4:03 pm
by Richard Blummer
WOW! That's beautiful work, Tim!

Re: Almost There
Posted: Fri Sep 07, 2012 4:14 pm
by Morganica
Looks great. Are you casting them together (or recasting with inclusions), or casting the pieces separately and gluing them in?
Re: Almost There
Posted: Fri Sep 07, 2012 4:57 pm
by Yardic Glassworks
Each of the characters, the barrel and the box are cast individually, then placed onto a wax base, reinvested, wax out, clear glass in.... so the piece is one solid piece, no glue. Tim
Re: Almost There
Posted: Fri Sep 07, 2012 5:09 pm
by Barry Kaiser
Beautiful and very well done.
Barry
Re: Almost There
Posted: Fri Sep 07, 2012 10:45 pm
by twin vision glass
Re: Almost There
Posted: Sat Sep 08, 2012 6:43 am
by Haydo
I'd guess that the first practice model has you fairly excited about where it can take you, I like it. From memory this is part of the natural progression in your work, would be great to see it all at some stage when the time is right. I'm looking at the work and see how it would create much enjoyment in all the processes. peace, haydo