Here are images of the uranium glass samples that I tested.
You're looking at pieces of uncut sheet and a small piece of three layers of fused sheet. I fired the 3 layers twice. The first firing was to a fire polish with no color change. the glass retained it's bright yellow-green color. The second firing of this same 3 layer piece was to a full fuse and as you can see the glass did strike to a whitish-yellow. A color which is not unpleasing.
Images:
1. Transmitted light. The edges of this glass have a strong yellow green color.
2. Reflected light. Appears milky.
3. Fused piece with strong back lighting.
4. Fused piece set on reflective aluminum with strong overhead lighting 4 feet away from glass.
http://photos.yahoo.com/bc/artistefem/l ... view=t[url][/url]
Uranium Glass Tests
Moderator: Brad Walker
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Uranium Glass Tests
GaleGale aka artistefem wrote:Here are images of the uranium glass samples that I tested.
You're looking at pieces of uncut sheet and a small piece of three layers of fused sheet. I fired the 3 layers twice. The first firing was to a fire polish with no color change. the glass retained it's bright yellow-green color. The second firing of this same 3 layer piece was to a full fuse and as you can see the glass did strike to a whitish-yellow. A color which is not unpleasing.
Images:
1. Transmitted light. The edges of this glass have a strong yellow green color.
2. Reflected light. Appears milky.
3. Fused piece with strong back lighting.
4. Fused piece set on reflective aluminum with strong overhead lighting 4 feet away from glass.
http://photos.yahoo.com/bc/artistefem/l ... view=t[url][/url]
Lots of different looks for one glass.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact:
Yes..........it's a very interesting multi-face, multi-use glass and when you look at it under a black light, it becomes even more interesting. Intense bright glowing green. Takes me back to my daze in the 60's-LOL!
My husband -god love him- sent a glow in the dark toilet seat to our son-in-law for Christmas. Don't ask - it's a guy bonding thing............
Our son -in-law also collects paintings on velvet. His latest kitsch art aquisition is a full rig semi-truck painted on velvet (2.5ft x 5ft) with plug-in running lights poking through the velvet. Very ni-e-e-e-e-ce.
I now know what to give for the next gift giving - hand-made glass glow in the dark matching bathroom accoutrement. Good news is with all the glowing going on in the bathroom, for those midnight runs to the potty - you would never miss the seat again or fall through when the seat is up!
Lordy, this could be a whole new niche in glass object making - LOL!
My husband -god love him- sent a glow in the dark toilet seat to our son-in-law for Christmas. Don't ask - it's a guy bonding thing............
Our son -in-law also collects paintings on velvet. His latest kitsch art aquisition is a full rig semi-truck painted on velvet (2.5ft x 5ft) with plug-in running lights poking through the velvet. Very ni-e-e-e-e-ce.
I now know what to give for the next gift giving - hand-made glass glow in the dark matching bathroom accoutrement. Good news is with all the glowing going on in the bathroom, for those midnight runs to the potty - you would never miss the seat again or fall through when the seat is up!
Lordy, this could be a whole new niche in glass object making - LOL!
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact: