Page 1 of 1

stainless floral former

Posted: Sat Sep 29, 2012 11:39 pm
by archie
I just bought a cple of new stainless floral former and Hitemp1800
Sprayed them, fired them to 700.
Put glass on when cold, set in kiln with some that I have had for years, the glass on new former stuck and broke, older ones were fine.
Any ideas?
tks

Re: stainless floral former

Posted: Sun Sep 30, 2012 1:35 pm
by Bert Weiss
poor coverage of the BN? Sandblast the steel clean and try regular kiln wash, a few coats.

Re: stainless floral former

Posted: Sun Sep 30, 2012 3:10 pm
by archie
thankyou
will try

Re: stainless floral former

Posted: Sun Sep 30, 2012 3:18 pm
by bob proulx
I agree with Bert, sandblast and use kiln wash.
Bob

Re: stainless floral former

Posted: Sun Sep 30, 2012 8:25 pm
by Tony Smith
I always put a slightly oversize disc of fiber paper over the end of the floral former. Just a bit paranoid about the glass getting stuck.