glass bottle frit
Can I use colored glass bottles to make frit and fuse into small objects.
I will not be mixing this bottle frit with other glass.
I will not be mixing this bottle frit with other glass.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: glass bottle frit
No. No you may not. You may not bring any bottles into your glass studio and pretend to make them into art.
Oops. Did I just say that out loud? Sorry; not a fan of melted bottles.
Do something spectacular and prove me wrong. : )
Oops. Did I just say that out loud? Sorry; not a fan of melted bottles.
Do something spectacular and prove me wrong. : )
-
williamslaybaugh
- Posts: 30
- Joined: Mon Mar 12, 2012 9:07 am
- Location: San Diego
Re: glass bottle frit
Yes you can and most bottle colors are compatible not only with other bottles but with float glass (Do some testing). It's a good cheap way to learn your craft, the art will come later.
Re: glass bottle frit
It's a nice way to practice, yes, but I disagree with the "compatible not only with..." part of this statement. In my experience float and random bottles are maybe compatible, maybe not. Your piece may fail because the glass isn't compatible, or for some other reason. The uncertainly makes it harder to figure out why and learn from your failures. If you're going to go this route, try initially confining your pieces to smallish ones, so that you only use one kind of glass in a single piece.williamslaybaugh wrote:Yes you can and most bottle colors are compatible not only with other bottles but with float glass (Do some testing). It's a good cheap way to learn your craft, the art will come later.
Or start by learning to test for compatibility, then doing those tests on new batches of glass. Personally, I think bottles don't yield enough glass to justify the testing, especially since manufacturers can buy their containers from multiple sources. There's no guarantee that this batch of, say, juice bottles, will work with the same bottles from another batch.
I've seen some pretty spectacular work done with scrap glass, though, so it's worth playing around with it.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Beau Lyons
- Posts: 32
- Joined: Fri Sep 21, 2012 11:47 pm
Re: glass bottle frit
ok, so I can use my left over alcohol bottles, So what is an inexpensive way to color clear glass (from broken bottles)
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: glass bottle frit
Enamels will give colour. However, they are not cheap. Not much in kiln forming is.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Beau Lyons
- Posts: 32
- Joined: Fri Sep 21, 2012 11:47 pm
Re: glass bottle frit
Hi Stephen,
I had a look at your web site, very good, a shame i am on the other side of the world.
When you say enamels, can you explain a bit more, what type of store would sell them over here.
regards, beau
I had a look at your web site, very good, a shame i am on the other side of the world.
When you say enamels, can you explain a bit more, what type of store would sell them over here.
regards, beau
Re: glass bottle frit
Beau, it sounds as though you need a couple of good reference books. Brad, the owner of this WGB wrote one. There are others too, that will give you the basics. Classes are given in some of the major cities here and in some smaller towns, by glass retailers.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: glass bottle frit
also the free tutorial is a great way to get started. helps with jargon as well. rosanna
artist, owner of wanchese art studio, marine finisher