Effetre 104coe Bullseye 90 coe rods
Posted: Fri Oct 26, 2012 9:57 pm
				
				I have been using Bullseye glass for beads recently. I wanted to combine some torchwork items with fused Bullseye pieces.
I was not diligent enough in keeping BE and Effetre rods completely separate.
I recently have some beads that cracked, and when trying to figure out which rod was the culprit, I think the Effetre rods are a bit larger. The Bullseye seems to be thinner.
Can anyone share their opinion please?
(But be gentle, I know I screwed up..., again)
I know I can always test for compatibility.
			I was not diligent enough in keeping BE and Effetre rods completely separate.
I recently have some beads that cracked, and when trying to figure out which rod was the culprit, I think the Effetre rods are a bit larger. The Bullseye seems to be thinner.
Can anyone share their opinion please?
(But be gentle, I know I screwed up..., again)
I know I can always test for compatibility.