Re-Priming Kiln Shelf
Posted: Thu Nov 29, 2012 7:39 pm
I am re-priming my kiln shelf. I used dry wall sand paper and took off the old primer and started fresh. I put 6 coats of Bullseye primer on and the primer starting bubbling up in places and flaking off. Is this normal? I have primed 2 kiln shelves and several molds and this is the first time it has happened.