Page 1 of 1
hmmmm.....cookie press?
Posted: Thu Dec 06, 2012 3:27 pm
by Laurie Spray
I wonder if this would work well for powder mixed with medium..
Any tried something like this for decorative elements? faster than freeze method??
http://www.surlatable.com/product/PRO-6 ... orage-Case
Re: hmmmm.....cookie press?
Posted: Thu Dec 06, 2012 4:03 pm
by Tracy Fries
How cool would that be? Would love to know if anyone has had success with this - especially since it has been years since my press has actually been used for cookies!
Re: hmmmm.....cookie press?
Posted: Thu Dec 06, 2012 9:52 pm
by Barry Kaiser
Have tried similar things. The problem is the liquid squeezes out in the first one or two and then you are left with what approaches cement in the gun.
Barry
Re: hmmmm.....cookie press?
Posted: Fri Dec 07, 2012 9:53 pm
by Laurie Spray
interesting Barry........I wonder if that would happen if you mixed it and used it all immediately.....
not looking for cement thats for sure.