plaster
Moderators: Brad Walker, Tony Smith
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
plaster
What is the best release for a plaster mold taken off of a plaster master? I have lost one and do not want to lose another!!!! Thanks!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Re: plaster
I have used several alternatives..
Liquid soap is a good one.
If the piece is dry enough, any oil works well.
On a wet surface oil may separate and leave gaps.
Even a slurry of clay may work, if you manage to open when it is still wet.
It is the most difficult, as it deters air flowing into the seam. It also tends to mask details.
Liquid soap is a good one.
If the piece is dry enough, any oil works well.
On a wet surface oil may separate and leave gaps.
Even a slurry of clay may work, if you manage to open when it is still wet.
It is the most difficult, as it deters air flowing into the seam. It also tends to mask details.
-
Jim Murphy
- Posts: 28
- Joined: Mon Mar 10, 2003 12:39 pm
- Location: IL
Re: plaster
Hi Laurie, typically a plaster master is first sealed with a suitable liquid soap [e.g. green tincture soap, or Murphy's Oil Soap], thenLaurie Spray wrote:What is the best release for a plaster mold taken off of a plaster master? I have lost one and do not want to lose another!!!! Thanks!
a release is applied such as vaseline or commercially available silicone emulsion.
Plaster-on-plaster though may be impossible if there are undercuts. Enter rubber moldmaking to the rescue!
Good luck!
Jim
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: plaster
spray paint the plaster and then use the above suggestions.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: plaster
Thanks.....no undercuts.....all good ideas.
Never thought of paint first. So that sort of seals the plaster?
Never thought of paint first. So that sort of seals the plaster?
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: plaster
Thin clay slip (very watery clay) is the best. Nothing beats it.
Paint the thin clay slip on, then immediately apply the plaster. Wait until the plaster hardens then dunk the whole lot in water. Wait a little while and it will separate out easily.
Paint the thin clay slip on, then immediately apply the plaster. Wait until the plaster hardens then dunk the whole lot in water. Wait a little while and it will separate out easily.
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Re: plaster
Thanks Peter,
as a self tought, or really by reading a lot.
I have had trouble with the clay slip, because i had not learned
the "dunk in water phase.
-lauri
as a self tought, or really by reading a lot.
I have had trouble with the clay slip, because i had not learned
the "dunk in water phase.
-lauri
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: plaster
spray paint/laquer and silicone spray over that. rosanna
artist, owner of wanchese art studio, marine finisher
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: plaster
Hmmmmmm.....dunk in water.......so do you "dunk" the mold then paint on the slip? Let it dry then spray? Interesting. I never hear about the dunk!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: plaster
One trick I have seen used, is compressed air. You blow strong air at the seam and it gets in there and pushes the pieces apart. Of course, this assumes you used an effective separator system. I was impressed by this, as the 2 parts were not going to just pull apart by hand. I saw this done at Pilchuck.
I am a big fan of rubber molds. They are relatively easy to work with, flexible, and can be forgiving. I have worked with rubber molds, with undercuts, that did break the plaster. If you need a forgiving mold, thin rubber backed up with plaster, for stability can work.
I am a big fan of rubber molds. They are relatively easy to work with, flexible, and can be forgiving. I have worked with rubber molds, with undercuts, that did break the plaster. If you need a forgiving mold, thin rubber backed up with plaster, for stability can work.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: plaster
Compressed air works, slip works better (especially if you first apply butchers wax or liquid soap and THEN apply the slip).
Personally, I'm not a huge fan of plaster to plaster mold making. Plaster masters have very little tolerance for undercuts or even 0-drafts so I typically wind up re-engineering the model for plaster (and given the number of undercut details I typically use, that's a major headache). Plaster molds can be heavy and awkward to work with once you're working with larger pieces, they're fragile to store and I always seem to knock them at exactly the right angle to pop off a detail, so they don't seem to last.
I much prefer using flexible RTV silicone/urethane for a master mold. If I'm trying to make a positive mold (i.e., a mold of a mold), I'll make the negative with elastack. It's a remeltable flexible mold material (rather like Gelflex from the UK, or composimold). Then I pour the silicone into the elastack mold, pull it out, and melt the elastack back down.
(On the plus side, plaster molds are cheap and they make great wax molds--wax poured into a wet plaster mold has a beautiful surface and if you dunk the whole plaster in water the wax will float right out)
Personally, I'm not a huge fan of plaster to plaster mold making. Plaster masters have very little tolerance for undercuts or even 0-drafts so I typically wind up re-engineering the model for plaster (and given the number of undercut details I typically use, that's a major headache). Plaster molds can be heavy and awkward to work with once you're working with larger pieces, they're fragile to store and I always seem to knock them at exactly the right angle to pop off a detail, so they don't seem to last.
I much prefer using flexible RTV silicone/urethane for a master mold. If I'm trying to make a positive mold (i.e., a mold of a mold), I'll make the negative with elastack. It's a remeltable flexible mold material (rather like Gelflex from the UK, or composimold). Then I pour the silicone into the elastack mold, pull it out, and melt the elastack back down.
(On the plus side, plaster molds are cheap and they make great wax molds--wax poured into a wet plaster mold has a beautiful surface and if you dunk the whole plaster in water the wax will float right out)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: plaster
Thanks! I do know the air compressor trick. My problem project was pottery plaster to pottery plaster with mold soap in between....... Obviously i will do more next time! Mold soap alone did not work. 
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: plaster
Well, the big deal is the what you're making the mold of...if neither side is flexible, really watch your shapes.Laurie Spray wrote:Thanks! I do know the air compressor trick. My problem project was pottery plaster to pottery plaster with mold soap in between....... Obviously i will do more next time! Mold soap alone did not work.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: plaster
It is shallow with no undercuts...just some subtle texture...should be so easy. I will be doing it again today with suggestions from here!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com