Page 1 of 1

Streaky glass effect

Posted: Wed Apr 17, 2013 6:45 pm
by Peter Angel
Hello. This is a stained glass window by Harry Clarke.
tumblr_mk2nmiqjTP1rqygz0o1_500.jpg
See the streaks in his hooded cloak? I like this effect.

Is it part of the texture in the glass itself or is it kiln fired enamel/glass paint?

Peter

Re: Streaky glass effect

Posted: Wed Apr 17, 2013 7:39 pm
by Marty
paint.

google drapery glass.

Re: Streaky glass effect

Posted: Wed Apr 17, 2013 9:53 pm
by Bert Weiss
Acid etched red flashed glass. I could verify that if I was looking at it. Red flashed glasses are stunning looking, and no vitreous enamel has that look.