I have just completed a new tutorial on the "Pattern Bar Flow Technique". Thought I would share it here. It is too much fun! We have just barely dented the surface on the fun possibilites of this technique and I am loving it!
http://www.igrowhydro.com/fusedglassart ... hnique.pdf
http://www.igrowhydro.com/fusedglassart ... hnique.pdf
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: New tutorial
Cool look and so easy!!
Barry
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
Re: New tutorial
Going to try it with my 12 !/2" SS round from Laurie !
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: New tutorial
Thank you for sharing the info, Laurie. I particularly like the design of the piece in the very last picture (love the color purple).
Dana W.
Dana W.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: New tutorial
These pictures are just some starters learning the weights and fusing programs. It has opened my mind to lots and lots of new possibilities! I have had a HUGE email response today from customers that are so excited! Really fun! Soon I will have all the weights calculated to make it even easier! I will add more pictures to the tutorial on our site as they come out of the kilns. 
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Eric Baker
- Posts: 51
- Joined: Thu May 20, 2004 9:19 am
- Location: Owasso, OK
Re: New tutorial
Those are fun, and a lot of possibilities exist. I had a similar idea a few years back with some scrap pattern bar pieces, but never followed up--just left it sitting in the 'try it someday' pile.
Now I'll brush off the dust and go with the 'flow'.
Thanks for sharing, Laurie.
warm regards,
Eric
Now I'll brush off the dust and go with the 'flow'.
Thanks for sharing, Laurie.
warm regards,
Eric
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: New tutorial
Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: New tutorial
Beautiful, Laurie.Laurie Spray wrote:Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!
I ordered a new tile saw (MX-370exp) that should arrive early this next week. Can't wait to get cutting!
Dana W.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: New tutorial
I just got a "brutus". i Love it!!!
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: New tutorial
I just got a "brutus". i Love it!!!
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
http://www.amazon.com/QEP-61024-24-Inch ... s+tile+saw
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Mark Wright
- Posts: 49
- Joined: Mon Dec 13, 2010 12:43 pm
- Location: Raleigh, NC
Re: New tutorial
This is great fun!
Thanks Laurie.


Thanks Laurie.


Re: New tutorial
Mark that's great!!!! Well done!
I'm going to start playing with bars over the summer.
I'm going to start playing with bars over the summer.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: New tutorial
Very addictive.........so much fun to do something new!!!!
Thanks for posting the pictures!!
Thanks for posting the pictures!!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com