howdy all ,,i am going to have a go at using a drop ring hope to make a small vase the ring has a top of 5.5" wide, the hole 3 " and hope to get a drop of about 5" to 6 ". so here is the question ,will be using 3mm glass ,,how many layer should i fuse together for the blank (am thinking 4),,and will it mater a great deal if i end up with a few air bubbles in the blank as some of the glass is a heavy texture,,all so should i put a clear layer over iridised glass..many thanks

Re: drop rings
Posted: Tue May 07, 2013 11:16 pm
by Barb R
I always follow Brad's advise as was stated in this Warmtip:
http://www.warmtips.com/20050808.htm
Barb
Re: drop rings
Posted: Wed May 08, 2013 4:08 am
by seachange
I made a couple of small vases last year, just to try. The small air bubbles elongate into thinnish lines.
I thought i should spend a lot more time improving the blank, but when people saw the vases, everyone commented, to my surprise, that they loved the air bubbles.
Good luck with your project, seachange
Re: drop rings
Posted: Wed May 08, 2013 11:45 pm
by Paul Schulz
OMG i didn't realizes all that info was in this site,,,Bard you are a walking encyclopedia ,,that much of taken you years to put together,,,THANKYOU just doesn't seem to say it some how