Page 1 of 1
fusing Wafers
Posted: Sat Jun 15, 2013 10:28 pm
by TerriSpiteri
I'm pretty new to fusing, but have taken a couple classes using glass powder and making wafers. I trying to fuse the wafers to solid glass, and am having trouble coming up with a good fusing schedule. Any suggestions?
Thanks
Terri
Re: fusing Wafers
Posted: Sun Jun 16, 2013 2:10 am
by Stephen Richard
Try out the education section of the Bullseye Glass site. There is a lot of good information there that will apply to all fusing glasses, although temperatures may need to be tweaked.
http://www.bullseyeglass.com/all-methods.html
Brad gives good information in the tutorial on this site that will be applicable.