Spectrum & Bullseye Clear Fusible Glass
Moderators: Brad Walker, Tony Smith
-
rainbowsoup
- Posts: 1
- Joined: Tue Feb 10, 2004 3:13 pm
- Location: Phoenix AZ
- Contact:
Spectrum & Bullseye Clear Fusible Glass
Greetings. I have a small problem relating to Bullseye and Spectrum Clear Fusible Glass. I work with both brands of glass. In one of my more addled states I cut up a sheet . Now two months later, I'm trying to figure out what it is. Spectrum? Bullseye? The clear fusible glasses look the same.
Is there a visual test that I can do besides test fusing? Thanks much. Paula
-
Wallace Venable
- Posts: 38
- Joined: Sun Mar 09, 2003 8:34 pm
- Location: Morgantown, WEST Virginia
- Contact:
Well, yes, if its NEW glass the Spectrum is flat and 96 COE while the Bullesye is textured and 90 COE.
The possible gotcha is that Bullseye used to sell very flat double rolled 90 which were reported produced by Spectrum under contract. (Sigh - I loved the 12 x 12 inch sheets of this glass)
The possible gotcha is that Bullseye used to sell very flat double rolled 90 which were reported produced by Spectrum under contract. (Sigh - I loved the 12 x 12 inch sheets of this glass)
Wally Venable, Student of glass
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
And, as if that isn't complicated enough, Bullseye also sells (or used to sell, or might sell, or something) clear that's made by Wissmach. (1110-83, and I believe it's smoother than regular BE clear.)Wallace Venable wrote:The possible gotcha is that Bullseye used to sell very flat double rolled 90 which were reported produced by Spectrum under contract. (Sigh - I loved the 12 x 12 inch sheets of this glass)
And, just to make it more interesting, you can also buy clear 90COE from Uroboros which is just as smooth as the old clear that Spectrum made for Bullseye. It might be (or it might not be, damned if I know) made for Uroboros by Spectrum.
If you think this is entertaining, try to figure out where a Toyota is made.
-
Cynthia
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Well, that's where it was assembled. But I bet the parts were made somewhere else.Cynthia wrote:Mine was proportedly made in Kentucky. I think that is just north of Kyoto. My VW is made in Wolfsberg...is that anywhere near Kentucky?Brad Walker wrote:...If you think this is entertaining, try to figure out where a Toyota is made.
A few years back I wanted to buy a Honda Accord. The dealer offered me a choice of two: one was assembled in Ohio, one was assembled in Japan. They were identical and had the same warrenty, but the one made in Ohio was a "new" car and the one made in Japan (which had 17 miles on the odometer) had been imported as "used." So much for quotas.
I bought the used car for $1000 less. That about 13,000 yen.
-
gone
Re: Spectrum & Bullseye Clear Fusible Glass
I can only answer as if I were you Paula and say I would do a test firing to check compatibility. The glass I make will outlive me so an extra day to check it's the correct glass is but a drop in the pond.rainbowsoup wrote:Greetings. Is there a visual test that I can do besides test fusing? Thanks much. Paula
I drive a Honda, built in UK, goes like a rocket. They call it Stevenson's rocket.
It ain't where you're from, it's where you're at!
-
Marilyn Kaminski
- Posts: 22
- Joined: Wed Mar 12, 2003 10:27 am
- Location: Boulder, CO
In issue #61 of Stained Glass News there is an article by Gil Reynolds. Part of the article tells how to identify the glass manufacturer by looking at the edge of the glass. If you're not sure of the color from the edge, stack three of four pieces together, the color will be stronger.
When viewed from the edge:
Window glass (or float) will have a dark green cast.
Bullseye tends to be light gray.
Spectrum 96 has a light yellow green hue.
Standard Spectrum is light blue.
Uroboros 90 and 96 have a yellow green color.
But still the safest way is to fuse a test piece and use polarizing film.
Hope this helps.
Randy
When viewed from the edge:
Window glass (or float) will have a dark green cast.
Bullseye tends to be light gray.
Spectrum 96 has a light yellow green hue.
Standard Spectrum is light blue.
Uroboros 90 and 96 have a yellow green color.
But still the safest way is to fuse a test piece and use polarizing film.
Hope this helps.
Randy
When injustice becomes law, rebellion becomes duty.
-
Lynne Chappell
- Posts: 186
- Joined: Fri Mar 14, 2003 2:05 am
- Location: Surrey B.C. Canada
- Contact:
"Spectrum 96 has a light yellow green hue.
Uroboros 90 and 96 have a yellow green color."
Yes, it's virtually impossible to be sure. And there is an inconsistency here in that the machine rolled clear with the Uroboros label is 90, the 96 has a Spectrum System 96 label on it. There were color differences between the machine rolled glass that Spectrum made for Bullseye and the glass they are still making for Uroboros, even they were both 90. And all of it that is in my rack right now looks sort of yellow (90 and 96). I don't think that the color is totally consistent over the years either. Test your glass. And in the future, label each and every piece of glass with permanent pen as you cut it.
Uroboros 90 and 96 have a yellow green color."
Yes, it's virtually impossible to be sure. And there is an inconsistency here in that the machine rolled clear with the Uroboros label is 90, the 96 has a Spectrum System 96 label on it. There were color differences between the machine rolled glass that Spectrum made for Bullseye and the glass they are still making for Uroboros, even they were both 90. And all of it that is in my rack right now looks sort of yellow (90 and 96). I don't think that the color is totally consistent over the years either. Test your glass. And in the future, label each and every piece of glass with permanent pen as you cut it.