I have done about 10 firings on my kiln and have not always needed to put kiln wash on the shelf each time. My last firing which was a bottle slumping put some indentations in the kiln wash when the bottles were removed and made it uneven. I tried to clean all of the wash off the kiln shelf and redo it but had a hard time removing it so I decided to flip the shelf over and use the other side.
So I don't build up a "kiln wash crust" again, I am wondering if I am supposed to completely clean the kiln wash off after each firing and reapply?
Kiln Wash Crust
Moderator: Tony Smith
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Kiln Wash Crust
You can get quite a few loads done with one application of kiln wash. When it starts chipping off it is time to remove it. I use a hand sander with rough sand paper until it is completely gone. The shelf just gets smoother and smoother. Be sure to wear a mask. It can be a dusty job.
When doing something extra hot like pot melts I sand it down with each firing and reapply fresh.
When doing something extra hot like pot melts I sand it down with each firing and reapply fresh.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Kiln Wash Crust
drywall sanding mesh
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Kiln Wash Crust
The hotter you fire, the less durable is the kiln wash. Keep your firings under 1400ºF, and it will last a very long time. I advise at least a thin fresh coat after you have fired over 1400. Many times you can get away without this, but sometimes a white scum is left. I hate it when that happens. As others said, when you fire hot, you want a good fresh coating. After it has chipped, the only way to get rid of the ridge is to remove it all. I like Kevin's open mesh sanding screen as the most effective abrasive that doesn't get clogged up.
I use a bit different strategy. For firings above 1400, I make my own kilnwash mixing about 80% finely ground alumina hydrate with 20% EPK, by weight. This mixture is pretty easy to clean off each time. I work primarily with float glass, which requires a thinner coating than the fusing glasses. When I work on hard shelves, I usually paint a pattern on with my kilnwash which leaves a decorative imprint. For most of my flat shelf work, I fire on fiber board that has been dusted with alumina hydrate, and no wet kiln wash. Much of my work is done on the kiln floor with either a sandbed or powdered fiber blanket. These are the easiest approaches for me, in my kilns.
I use a bit different strategy. For firings above 1400, I make my own kilnwash mixing about 80% finely ground alumina hydrate with 20% EPK, by weight. This mixture is pretty easy to clean off each time. I work primarily with float glass, which requires a thinner coating than the fusing glasses. When I work on hard shelves, I usually paint a pattern on with my kilnwash which leaves a decorative imprint. For most of my flat shelf work, I fire on fiber board that has been dusted with alumina hydrate, and no wet kiln wash. Much of my work is done on the kiln floor with either a sandbed or powdered fiber blanket. These are the easiest approaches for me, in my kilns.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions