				easy to make sifter
				Posted: Sat Jul 06, 2013 6:48 pm
				by Paul Schulz
				while i'm sure this has been done before,, i'm all so sure, that there are newbies like my self who would like this,,the photos say it all just make sure the cloth is a very fine weave ,and hold it tight as you screw the top back on
			 
			
					
				Re: easy to make sifter
				Posted: Sun Jul 07, 2013 12:40 pm
				by Vicki M
				Thanks for posting, I wouldn't have thought of doing that. Good tip.
			 
			
					
				Re: easy to make sifter
				Posted: Sun Jul 07, 2013 4:51 pm
				by Barry Kaiser
				Actually your timing was great. I am working on a project that it will be very useful.
Thanks Paul.
Barry
			 
			
					
				Re: easy to make sifter
				Posted: Sun Jul 07, 2013 7:01 pm
				by Kevin Midgley
				RESPIRATOR!!!!
			 
			
					
				Re: easy to make sifter
				Posted: Sun Jul 14, 2013 4:03 am
				by seachange
				Many thanks Paul, it will become very useful.