Page 1 of 1

copper tube

Posted: Sun Jul 21, 2013 7:31 pm
by Paul Schulz
hi guys,, can someone tell me if i can use copper pipe as a mould for laying glass over, for glass weaving . i realize i'll have to use kiln paper or kiln wash , but am not sure if the pipe will distort too much. would only be taking the temp to 700c and as copper melds at 1085c it should be OK

many thanks paul

Re: copper tube

Posted: Sun Jul 21, 2013 8:27 pm
by Kopperwood
The copper will anneal and go dead soft around 1000 F and will bend easily if it is small. That may or may not be a problem, just wanted you to be aware of it.

Perry

Re: copper tube

Posted: Mon Jul 22, 2013 6:36 am
by rosanna gusler
It will also spall like crazy and can stain your shelf. It also might cause reactive glasses to react. R.

Re: copper tube

Posted: Mon Jul 22, 2013 5:55 pm
by Paul Schulz
ah i hadn't thought of it reacting,,,i'll use an old shelf,,thanks guys for the info