schedule for 50X25 piece, 6 mm thick

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Carol Ann
Posts: 29
Joined: Tue Nov 18, 2003 11:52 am

schedule for 50X25 piece, 6 mm thick

Post by Carol Ann »

never fired a piece this large before, need some advice as to schedule for firing.
thanks
Carol Ann
Jerrwel
Posts: 129
Joined: Thu Feb 10, 2005 6:25 pm
Location: Charlotte, NC

Re: schedule for 50X25 piece, 6 mm thick

Post by Jerrwel »

Carol Ann wrote:never fired a piece this large before, need some advice as to schedule for firing.
thanks
http://www.warmglass.org/books/books/126-fsg
Jerry
Carol Ann
Posts: 29
Joined: Tue Nov 18, 2003 11:52 am

Re: schedule for 50X25 piece, 6 mm thick

Post by Carol Ann »

thank you Jerry i will look into the book you suggested.