Kiln wash won't stick to new ceramic mold
This is the first time I've encountered this problem. I was putting kiln wash on some new molds tonight. One of the molds the kiln wash beads up. These are ceramic molds like all the rest that I have. I mean it kinda sticks but I can brush it off in areas. It's like there's something on the mold yet I can't see or feel anything. What is the problem? Help help. 
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Kiln wash won't stick to new ceramic mold
There might be some oil or residue on the mold.
Perhaps firing it in your kiln to a low temp might burn the oil off? Washing it with soap and water might work as well.
Perhaps firing it in your kiln to a low temp might burn the oil off? Washing it with soap and water might work as well.
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Kiln wash won't stick to new ceramic mold
i would fire it to 1000f or just put it in with whatever firing you do next. if that does not help then what you have is a result of how the mold was poured. the clay can be compressed in an area and less able to easily hold kw.
artist, owner of wanchese art studio, marine finisher
Re: Kiln wash won't stick to new ceramic mold
If it's still doing that after firing you can sometimes fix it by sanding the area. I use a coarser grade of sandpaper and bear down a bit. That gives the area a little tooth so the kilnwash can adhere. Doesn't always work, but it's worth a try. Any marks you make on the mold will be filled in with kilnwash, so it doesn't affect the texture.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Kiln wash won't stick to new ceramic mold
Thanks for the suggestions. I will give them a try! 
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Kiln wash won't stick to new ceramic mold
When they make molds with a "pour slip" method….where the slip hits is called a hard spot. It usually may look like it does not have kiln wash on it but it probably has some. I would lightly sand it or put it on a hot kiln, try again, and then use it!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com