Question: What do you use for a sprayer for BE Spray A? The unit that I got eons ago was in a glass container attached to a can with some kind of propellant in it.... that doesn't work any more. I've tried various misting sprayers from garden shops, and still haven't found one that gives a fine enough mist. Suggestions? Thanks!
Kim Bellis
Posts: 133
Joined: Sat Jun 14, 2003 9:48 pm
Location: Tampa, Florida
Contact:

Post by Kim Bellis »

I use a air spray gun. You can get them at any "hobby" store from inexpensive to expensive.
Kim
Mark Hughes
Posts: 49
Joined: Mon Mar 17, 2003 6:27 pm
Location: Omaha, Nebraska

Post by Mark Hughes »

I use an air brush hooked up to my air compressor with the pressure dialed down to about 10 lbs. It gives a nice fine spray. 8)
Mark Hughes
Valla E
Posts: 11
Joined: Tue Jan 06, 2004 3:20 am
Location: also on Salt Spring! British Columbia, Canada
Contact:

Post by Valla E »

Thanks! (still hoping for a cheaper alternative! :D )
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

you can get a mouth atomizer for very few dollars. you can get an air can propellant spray gun cheaply at hobby places (michaels, for instance).

i've seen a sprayer that can be hooked up to a scuba tank or a spare tire.
Valla E
Posts: 11
Joined: Tue Jan 06, 2004 3:20 am
Location: also on Salt Spring! British Columbia, Canada
Contact:

Post by Valla E »

Thanks for the tips! Michael's must have an online catalogue..... I'll check!
Scotty
Posts: 18
Joined: Tue Jun 24, 2003 9:48 am
Location: St. Pete., FL

Post by Scotty »

I bought a very inexpensive ($10) air brush from Harbor Freight.
Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Post by Lynn g »

Fusion HQ (see link above) has a quick-spray atomizer (mouth sprayer); the latest catalog I have says it's $8.50.
Valla E
Posts: 11
Joined: Tue Jan 06, 2004 3:20 am
Location: also on Salt Spring! British Columbia, Canada
Contact:

Post by Valla E »

Gee, thanks so much everyone! What a response! Hope I can return the favor sometime.. I really appreciate your taking the time to help me out on this! :D

Cheers!
Post Reply