Hello everyone. I am a Lampworker who is slowly getting into the wonderful art of fusing. Today a good friend of mine gave me a load of float glass. I have managed to get a good (I hope...) fusing schedule. However I simply can't find a schedule for slumping this glass into a mould. Does anyone have a slumping schedule for float. Obviously I understand the complexities of this glass and that each sheet could differ.....but a good basic start is all I require in centigrade please.
Thanks
Janey
Slumping schedule for float glass
Moderator: Tony Smith
Re: Slumping schedule for float glass
First- there's a temp conversion on this page.
Second- What kind of mold?
Second- What kind of mold?
-
Tammy Macdonald
- Posts: 15
- Joined: Tue Jun 18, 2013 1:45 pm
- Location: Texas
Re: Slumping schedule for float glass
http://glasswithapast.com/ has lots of information about float and/or recycled glass. It's worth checking out.
Good luck.
Good luck.