Page 1 of 1

Slumping schedule for float glass

Posted: Fri Dec 20, 2013 3:56 pm
by Lemonkitten
Hello everyone. I am a Lampworker who is slowly getting into the wonderful art of fusing. Today a good friend of mine gave me a load of float glass. I have managed to get a good (I hope...) fusing schedule. However I simply can't find a schedule for slumping this glass into a mould. Does anyone have a slumping schedule for float. Obviously I understand the complexities of this glass and that each sheet could differ.....but a good basic start is all I require in centigrade please.
Thanks
Janey

Re: Slumping schedule for float glass

Posted: Fri Dec 20, 2013 7:44 pm
by Marty
First- there's a temp conversion on this page.
Second- What kind of mold?

Re: Slumping schedule for float glass

Posted: Sat Dec 21, 2013 3:23 pm
by Tammy Macdonald
http://glasswithapast.com/ has lots of information about float and/or recycled glass. It's worth checking out.

Good luck.