Page 1 of 1
Blanket
Posted: Thu Jan 16, 2014 9:58 pm
by Yardic Glassworks
Recovered from the last piece; New piece going in for firing...
UPDATE: Final fuse done which left some texture on the edges, then slumped into the final blanket form. Note how the Steel Blue went back to the steel color at the lower slumping temp.
Re: Blanket
Posted: Thu Jan 16, 2014 11:33 pm
by Valerie Adams
Holy cow! I can't even imagine the patience a piece like this takes. Bravo!
Re: Blanket
Posted: Fri Jan 17, 2014 10:50 am
by pshash
It's beautiful!
Re: Blanket
Posted: Fri Jan 17, 2014 4:01 pm
by JestersBaubles
Stunning! What a lot of precision cutting!
Dana
Re: Blanket
Posted: Fri Jan 17, 2014 8:11 pm
by Diane Allen
Wow, that is awesome.
Re: Blanket
Posted: Fri Jan 17, 2014 8:21 pm
by twin vision glass
I love this piece and would love to see it up in lights.

Leslie
Re: Blanket
Posted: Sat Jan 18, 2014 11:44 am
by Laurie Spray
Love the subtle color choices!
Re: Blanket
Posted: Sat Jan 18, 2014 6:21 pm
by Drewcilla
Very nice, indeed.
Re: Blanket
Posted: Sun Jan 19, 2014 8:47 am
by bob proulx
Great piece, how much time do you have in this.
Bob
Re: Blanket
Posted: Sun Jan 19, 2014 11:25 am
by Labrador
Just lovely
Sophie
Re: Blanket
Posted: Sat Jan 25, 2014 12:44 pm
by Havi
ibid -
To all that been said above......
Why 'recovered'?
Havi
Re: Blanket
Posted: Sat Jan 25, 2014 8:22 pm
by Yardic Glassworks
Bob,
I didn't really keep track of the time involved, but it has a thousand or so pieces. It took 4 trips in the kiln.
Havi,
"Recovered" was what it felt like after the last piece I was working on never really came together the way I wanted it to. I like this one much better. Thanks everyone for the nice comments. Tim
Re: Blanket
Posted: Sun Jan 26, 2014 2:38 pm
by jim burchett
beautiful piece
Re: Blanket
Posted: Thu Feb 06, 2014 12:03 am
by Buttercup
That's amazing! What are the dimensions please Tim? About 24" x 24" ? Jen
Re: Blanket
Posted: Thu Feb 06, 2014 1:40 pm
by Yardic Glassworks
Dimensions are 20" by 15". Tim
Re: Blanket
Posted: Thu Feb 06, 2014 6:11 pm
by Buttercup
Thank you. Jen
Re: Blanket
Posted: Sat Feb 08, 2014 11:42 am
by Haydo
What an effort to get clean lines and than to slump into such a sexy organic image of a rug in the wind, that is very cool. Thank you. peace, haydo
Re: Blanket
Posted: Mon Feb 10, 2014 7:22 pm
by Sue Hunchuk
Breathtaking!