Best to put frit between 2 layers or on top?
Moderator: Tony Smith
-
Shelley Lewis
- Posts: 73
- Joined: Wed Dec 11, 2013 11:14 am
Best to put frit between 2 layers or on top?
I want to use a green translucent base, a clear cap, and use black opal frit (medium) for some detail elements. Where is the best place for the frit? This will be a full fuse and later slumped.
Re: Best to put frit between 2 layers or on top?
On top . . .
-
Shelley Lewis
- Posts: 73
- Joined: Wed Dec 11, 2013 11:14 am