Page 1 of 1
thick glass
Posted: Wed Feb 12, 2014 11:24 pm
by Dick
Hi. Does anyone have a source of thick clear glass? need about 20 pieces about 6" x8" in either 1" or 1.5 inches thick. Can be float. Not cost effective to make, plus I don't want lines from sheet glass.
Thanks
Dick
Re: thick glass
Posted: Wed Feb 12, 2014 11:41 pm
by Bert Weiss
There is 1" float, made somewhere offshore. I don't know a source. For 1.5", maybe you can get some Schott from HIS?
Re: thick glass
Posted: Thu Feb 13, 2014 6:33 am
by Tony Smith
Dalle de Verre glass is available from Kokomo in 8 x 12 x 1" in colors and clear
http://www.kog.com/more-glass/dalles.html
Tony
Re: thick glass
Posted: Thu Feb 13, 2014 3:51 pm
by Dick
thanks I will check it out
Re: thick glass
Posted: Sat Feb 15, 2014 12:22 am
by Rick Wilton
i've been fusing two pieces of 3/4 together to make 1.5" then cutting with a tile saw and fire polishing to achieve a thicker blank. You can see a fine line but it's not too noticeable.
Re: thick glass
Posted: Sat Feb 15, 2014 3:13 am
by williamslaybaugh
I've got a bunch of the Dalle de Verre glass in storage. I'm not sure if I have 20 clear, but I also have transparent blue, green and red. I can run up there mid-week and post some photos and let you know what I've got if your interested.