Page 1 of 1
					
				Question about a mold
				Posted: Fri Feb 14, 2014 11:02 am
				by loricrawford
				I see a drape mold for a mask that I'd like to try. It's a half face mold with the eye sections  open. How to you keep it that way (no glass across the eye openings). Being in Mardi Gras country I think I could make some cute masks but being a newbie am confused about this part. Any advice would be appreciated!
			 
			
					
				Re: Question about a mold
				Posted: Sat Feb 15, 2014 12:04 pm
				by Bert Weiss
				Stuff the open eyes with fiber blanket dipped in alumina hydrate or kilnwash. Drape over face molds are tricky.  If the glass cracks it was because the glass shrunk more than the mold while cooling.  If it doesn't crack, you are good to go...
			 
			
					
				Re: Question about a mold
				Posted: Mon Feb 17, 2014 7:08 pm
				by loricrawford
				Thank you Bert.