Has anyone actually pressed glass - I would like to stack pieces of glass on a sheet of clear and then press down on it with another kiln shelf or a weight of some kind while fusing. Rather funky but curious if anyone has tried this.
Thanks Margie C
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Pressed Glass

Post by Valerie Adams »

Sure; lots of folks have done it!

Paul Tarlow has written up a really nice tutorial:

http://www.fusedglass.org/learn/project ... ssed_glass
Margie C
Posts: 2
Joined: Mon Sep 15, 2008 10:59 am

Re: Pressed Glass

Post by Margie C »

Thanks Valarie I will check it out. Margie