Hi,
What is the best way to make 1/8 inch thick frit balls with a flat top (in other words, I need oval-shaped, flattened 'balls'...):
1- Make the frit balls (full fuse) then flatten them under a KW-coated dam that will fall onto 1/8 inch fiber paper strips during a 2nd full fuse
or
2- Make the flattened balls in one full fuse step by placing my small glass pieces under the KW-coated dam held onto the fiber strips.
I know option #1 will work. I am just not sure whether the edges of the 1/8 inch thick glass pieces (i.e., those not in contact with the dam & the kiln shelf) would round up in option#2. Trying to save energy!
Cheers!
Lucie
Frit balls with flat tops
Moderator: Tony Smith
Re: Frit balls with flat tops
Cut long octagons (or hexagons) and fuse them, but stop the fuse before they draw up completely into balls?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Brad Walker
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Frit balls with flat tops
Just curious -- after you make these flat-top balls, how will you use them?