Silk screen, powders.... enamels etc.

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Silk screen, powders.... enamels etc.

Post by Havi »

I never did silkscreen, even though I have been printing a lot. Mostly I printed collographs and etchings . I have a great etching press which I brought home upon returning from USa, years ago.

However, I also have a screen and a squeegee.


Can anybody tell me what emulsion do I need to use,
AND
how, or with what should I mix the glass powder, in order to pass it thru the screen???? :-k :-k

I want to do simple silk screen, not photographic


I'd be more than grateful, This is quite important to me.

Many thanks,
Havi

I
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
tbach
Posts: 33
Joined: Tue Jan 04, 2011 11:35 pm
Location: Hillsboro, Oregon

Re: Silk screen, powders.... enamels etc.

Post by tbach »

Check out Stacey Lynn Smith - works at Bullseye. She has developed a system of imagery which is achieved by sifting fine glass powdered frit through prepared silkscreens. The clarity of images and texture is dependent upon the firing temp used. Her work will spark your imagination. I have been told that she has a facebook page "Print & Glass" for "sifting" followers. Don't use Facebook, so I can't verify.

I use screenprinting - both enamels and powdered frit in most of my glasswork - for some reason I saw the connection immediately when I began fusing. The type of emulsion does not matter much . . . just that you are comfortable with timing in order to get a useable screen. It takes some hit and miss stuff to figure that out. Stacey uses screens in the 130 size range - with the finer screen material, only very small powder particles will fall through. I use mostly 110 - it works for me with both powder sifting and enamel printing. For very detailed work with enamels, much finer screens can be used - the 200 range. I have a gallery online if you're interested. http://www.tedbachglass.com

By the way - I love your work and your fearless pursuit of glass. I figure that a day without a mistake is a day without learning, so I am trying to become more fearless - after all, it's just a piece of glass.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Silk screen, powders.... enamels etc.

Post by Buttercup »

Havi, you may find your screen's thread count to be in metric, not threads per inch. That threw me right off for quite a while as the screen I bought only has a number on it. It doesn't say per square centimetre, which it turned out to be. Duh!!

Good luck with your new venture. Jen
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Havi »

Many thanks to you both,
Jen and Ted
Mean while, I watched BE's lesson about powder screening.

I want to do as simple as possible. I shall copy of course your enlightening remarks.

But I am going simpley to see if my screen allows the powder to pass thru it . If so - then the whole thing is simple and easy.

And if not

I shall have to find another compromise. My idea is to use any tools I have to create a better piece of art, not to work with tools for the sake of working with them.
I'll see.

Anyway,
Thanks a lot

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Silk screen, powders.... enamels etc.

Post by S.TImmerman »

Bullseye has at least 3 videos in their online teaching system about silkscreen.
i believe its 35.00 a year. They add new videos each month and you're able to view all the older ones. They posted a powder screening video 2 months ago. You can also ask questions about said videos via their blog.
Great stuff!
Shereen


http://www.bullseyeglass.com/all-methods.html
Mary Kay Nitchie
Posts: 21
Joined: Mon Mar 10, 2003 8:02 pm
Location: Portland, Oregon
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Mary Kay Nitchie »

Hi Havi,

If you have a subscription to Bullseye's videos, here is a non-emulsion method to prepare your screen:

Screenprinting on glass with hand-cut stencils:
http://www.bullseyeglass.com/forum/inde ... =14&t=4024

Best of luck!

Mary Kay
Mary Kay Nitchie
Bullseye Glass Co.
http://www.bullseyeglass.com
beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: Silk screen, powders.... enamels etc.

Post by beninfl »

It bothers me that Bullseye charges for this. Not really a particularly wonderful way to support the people who buy their glass, to charge them to see how to use it. I wish Bullseye would reconsider that. No other manufacturer I can think of charges you for ideas on using their products.
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Stephen Richard »

beninfl wrote:It bothers me that Bullseye charges for this. Not really a particularly wonderful way to support the people who buy their glass, to charge them to see how to use it. I wish Bullseye would reconsider that. No other manufacturer I can think of charges you for ideas on using their products.
I find the above statement breathtaking in its misunderstanding .
It is possible to discover how to use fusing glass from many sources. You don't have to pay if you don't want to.
The effort Bullseye put into research and education benefits the whole glass community
Approximately $3 per month is a small sum
Bullseye deserve some return for the effort of producing the videos, they are not a philanthropic organisation.
Education is not free. Think how much you pay for classes and courses.
No other fusing glass manufacturer does this kind of support.

There are many other comments that could be made, but this gives my initial thoughts
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Havi »

Thanks Mary Kay,
As a subscriber to your educational video's I actually saw this video yesterday, and it illuminated my way. I shall watch also the recommended video's concerning pigments that are there.

For the benefit of those who are following this thread, and for the sake of 'honesty' I must mention that in Brad's new book there is a whole chapter dealing with screening etc. There are also other books dealing with various other methods of printing on glass. [- and if you want the book, you have to pay for it, I guess :wink: - ]

Many thanks,
I just need to if my screen can really pass the powder , or the other way round can the powder go thru my screen.

Good night to you all,
and thank you for being there for me,

Havi
Wish me luck in painting an image on the screen..............
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Bert Weiss »

Havi, you can use the same media used for painting with powders, but mix the ink to a thicker consistency. There are advantages and disadvantages in using either oil based media or water miscible media. The standard oil based medium from decades past is no longer manufactured the same and the new one isn't as good to work with. It is known for holding the most pigment. When working with a water miscible medium, you want a slow to dry one, so it doesn't clog up your screen. You can slow drying by adding some glycerine. (here in the USA, you can purchase a small bottle of glycerine, for a reasonable price, at the Walmart pharmacy). One downside to the water based medium is that it can make soap bubbles as you work the squeegee back and forth.

You want to size the screen mesh relative to the powder particle size. When using onglaze colors which are finely ground, you can use a tight weave screen. When using Bullesye frits, you need a more open screen. I can't quote mesh sizes. I would consult with the frit manufacturer to get their recommended sizes.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
willy66
Posts: 1
Joined: Sat Oct 21, 2023 9:18 am

Re: Silk screen, powders.... enamels etc.

Post by willy66 »

Havi wrote: Sat Mar 15, 2014 6:12 pm I never did silkscreen, even though I have been printing a lot. Mostly I printed collographs and etchings . I have a great etching press which I brought home upon returning from USa, years ago.

However, I also have a screen and a squeegee.


Can anybody tell me what emulsion do I need to use,
AND
how, or with what should I mix the glass powder, in order to pass it thru the screen???? :-k :-k

I want to do simple silk screen, not photographic


I'd be more than grateful, This is quite important to me.

Did you also know that you can find silk-made hair protection like the durags from this link see this. These durags are so fashionable while serving their main purpose of protecting our hair from the harmful rays of the sun.

Many thanks,
Havi

I
It's great that you want to give silk screen printing a try! To get started with simple silk screen printing, you'll need some basic supplies, including emulsion and ink. Here's a brief guide to help you get started:

Emulsion: You can use a photo emulsion for screen printing, but since you mentioned you want to do simple silk screen without photography, a direct or water-based emulsion would be more suitable. These emulsions are easier to work with for hand-drawn or simple stencil designs.

Screen: Ensure your screen is clean and in good condition. It's best to use a mesh screen appropriate for the type of designs you plan to print. For simple designs, a lower mesh count (around 110-160 mesh) should work well.

Glass Powder: If you want to thicken your ink, you can use a screen printing thickener instead of glass powder. It's easier to work with and specifically designed for screen printing. Glass powder may not mix well with ink and can be challenging to get the right consistency.

Ink: Use screen printing ink, which is designed to pass through the screen and adhere to fabric or paper. There are various types of ink available, such as water-based and plastisol inks. Choose the one that suits your project and preferences.

Squeegee: Make sure your squeegee is in good condition. The size of the squeegee should match the size of your screen.

Here's a basic overview of the process:

Prepare your design: Create your design or stencil on a transparent or translucent material. You can use various techniques like hand drawing, stencils, or even cut vinyl.

Coat your screen: Apply the emulsion to your screen following the manufacturer's instructions. Let it dry in a dark area, preferably a drying cabinet or a dark room, to prevent exposure to light.

Expose your design: Place your design on top of the coated screen and expose it to light (if you want to use a design). This step can be skipped for simple silk screen without photography.

Wash the screen: Rinse the screen with water to wash away the unexposed emulsion, leaving your design on the screen.

Printing: Mix your ink with a screen printing thickener if needed. Then, place your screen on the material you want to print on, apply ink, and use the squeegee to pass the ink through the screen onto your material.

Drying: Let your prints dry completely before handling or stacking them.

Remember that practice makes perfect in screen printing, so don't be discouraged if your first prints aren't perfect. Good luck with your silk screen printing, and I hope you achieve the results you're looking for!
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Silk screen, powders.... enamels etc.

Post by Havi »

Many thanks, Willy 66,
The thing is that i was thinking of printing on GLASS, not paper or fabric.
Also I might have wanted to fire the glass. So I guess it needs to be taken to considreation while printing - lest it will burn out when being fired.

still, many thanks,
H
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
theanimallover
Posts: 59
Joined: Tue Jan 22, 2008 9:19 am
Location: The Sticks, England, UK

Re: Silk screen, powders.... enamels etc.

Post by theanimallover »

Did someone reply to your post 10 years later?
Did you then respond as if it was a day later?
:!: :shock:
Post Reply