Page 1 of 1

gold and silver enamels

Posted: Sun Mar 30, 2014 7:11 pm
by Jill Wilson
I'm looking for a silver enamel similar to Hanovia Gold, Thompson Gold, or Duncan Gold. in searching for the silver, I'm no longer finding the gold ones either. So, is there a silver liquid enamel? And, do I need to begin hoarding my remaining bottles of the above named gold ones?
There was a lot of conversation about the golds in the past, but I'm not finding them under search.

Re: gold and silver enamels

Posted: Mon Mar 31, 2014 9:46 am
by Bert Weiss
There are platinum and palladium for the silver color. Hereaus is now the premier manufacturer of precious metal lustres. There are also Chinese knockoffs.

Re: gold and silver enamels

Posted: Mon Mar 31, 2014 8:07 pm
by Valerie Adams
Unique Glass Colors makes a couple metallic paints that work fairly well and are very inexpensive. I'm hoarding my bottles of the real stuff!