Pot melt problem

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
colettecoad
Posts: 3
Joined: Fri Oct 25, 2013 2:30 pm

Pot melt problem

Post by colettecoad »

I tried pot melting for the first time. I used a small terracotta pot and a recommended firing schedule. When it was done there was melted glass in the pot and a stream of glass connecting the bottom of the pot to the glass in the mold below. What caused this? I really need help. Thanks.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Pot melt problem

Post by Buttercup »

I'm definitely not qualified to give advice but check this out:

http://www.warmglass.com/phpBB/viewtopi ... =2&t=39790

Have fun :D Jen
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Pot melt problem

Post by charlie »

not hot enough for long enough.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Pot melt problem

Post by Judd »

That's normal. You needed more heat and more time.
colettecoad
Posts: 3
Joined: Fri Oct 25, 2013 2:30 pm

Re: Pot melt problem

Post by colettecoad »

Thanks to all for the links and advice. I will try hotter and longer.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Pot melt problem

Post by Marty »

Got a peep hole? One quick glance will tell you whether it's done or not.