Page 1 of 1
					
				Bullseye 1015 - reacts with silver
				Posted: Thu Nov 13, 2014 5:40 pm
				by Risa
				This glass is supposed to react with silver foil and result in a gold finished look.
Has anyone tried this yet?  I bought a piece and don't know what to do with it, so I'd love to see other projects.
			 
			
					
				Re: Bullseye 1015 - reacts with silver
				Posted: Fri Nov 14, 2014 7:47 am
				by Kim Manley
				I've seen a box by Nathan Sandberg made with this glass.  He brought it to Aus. In October.  I don't have a photo but there is clearly a reaction.  Bullseye won't ship any to Australia yet so haven't tried it.
			 
			
					
				Re: Bullseye 1015 - reacts with silver
				Posted: Fri Nov 14, 2014 9:04 pm
				by Valerie Adams
				There was an artist showing photos of her testing that glass on the FB group called Fused Glass Fanatics. 
You can join the group and search for 1015; it'll bring up her photos.
			 
			
					
				Re: Bullseye 1015 - reacts with silver
				Posted: Sat Nov 15, 2014 1:15 pm
				by Andrea R
				Is 1015 new?
			 
			
					
				Re: Bullseye 1015 - reacts with silver
				Posted: Sat Nov 15, 2014 2:18 pm
				by Brad Walker
				Andrea R wrote:Is 1015 new?
1015 is Reactive Silver Clear.  Special production at the present time, but may be in their line down the road.
 
			
					
				Re: Bullseye 1015 - reacts with silver
				Posted: Sat Nov 15, 2014 2:30 pm
				by Andrea R
				Brad Walker wrote:Andrea R wrote:Is 1015 new?
1015 is Reactive Silver Clear.  Special production at the present time, but may be in their line down the road.
 
Thanks Brad think I will need to get some of that!!!