Page 1 of 1
					
				Tac fuse for pebbles
				Posted: Mon Nov 17, 2014 7:06 pm
				by byjoanna
				I remembered from something that I cover a circle with pebbles then tac and slump.  I have one layer circle and covered it with pebbles.  Need suggestions for firing schedule - I don't want to loose the texture but I want the pebbles to most definately be attached.  Thanks
			 
			
					
				Re: Tac fuse for pebbles
				Posted: Mon Nov 17, 2014 10:39 pm
				by rosanna gusler
				wont work. glass will break on cool dowd. r.
			 
			
					
				Re: Tac fuse for pebbles
				Posted: Tue Nov 18, 2014 7:12 pm
				by jim simmons
				Glass pebbles or  rock pebbles?
Glass will work, rocks will not.
Jim
			 
			
					
				Re: Tac fuse for pebbles
				Posted: Thu Nov 20, 2014 3:09 pm
				by Charlotte Kay
				I think she means fused glass "pebbles" that you make from breaking up a pattern bar or pot melt. Kinda like frit balls.
I have used either the 2-layer or the 3-layer fusing schedules for a tack fuse on fusedglass.org  Depends on how thick your base circle is and  how thick your pebbles are. You want to use the thickest measurement in your calculations.
			 
			
					
				Re: Tac fuse for pebbles
				Posted: Sun Nov 23, 2014 6:39 pm
				by Valerie Adams