Casting and Annealing over 20cm/8in
Posted: Sat Jan 03, 2015 1:26 pm
Hi all!
I'm about to cast a head with part of a chest where my thickest part is 23cm thick ...
Should I calculate a ratio based on the BE table (ending at 20cm) or are there any other ways?
Thanks!
Here are 2 pictures of the plaster model of the sculpture. It is a life size figure of a young boy - 1.55m tall. Most of it is to be bronze (already cast) and the head, the collar of the coat, the waistcoat and the shirt are going to be glass.
Lucho
I'm about to cast a head with part of a chest where my thickest part is 23cm thick ...
Should I calculate a ratio based on the BE table (ending at 20cm) or are there any other ways?
Thanks!
Here are 2 pictures of the plaster model of the sculpture. It is a life size figure of a young boy - 1.55m tall. Most of it is to be bronze (already cast) and the head, the collar of the coat, the waistcoat and the shirt are going to be glass.
Lucho