Are there any specific instructions as to how to work with vermiculite shelf, as opposed / different than mullite [ceramic?] boards???
My Dysson shelf broke, and the bigger shelf
I have is Verm. I wonder if I should do something different that the way I worked with the Dysson??
How long will the vermiculite last?
Do I have to worry about temperatures? not too high, maybe??? The shelf is appx. 1" thick.
I'd be grateful for your responses - - -
Many thanks in advance
H.
Vermiuculite board
Moderator: Tony Smith
Vermiuculite board
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Vermiuculite board
I have been using the same 1" Vermiculite shelf now for 8 to 10 years. Initially I painted rigidizer on both sides. Then I remeber the first firing with empty kiln was somewhat smokey (be prepared to vent studio).. One important step is always provide plenty of support underneath. I space mine up off kiln floor 3/4" with numerous blocks and strips from old kiln helves cut up. I do not kilnwash the shelf....instead I use thinfire or dry powder for textured underside. A 2' x 3' shelf is quite manageable to lift in and out to do your build-up on workbench. I have a second one I bought at same time as original and have never had to use it. The bonus is I can tack stainless steel pins thru fibreboard into shelf to build molds etc...dry powder fills in holes after.
"The Glassman"
Re: Vermiuculite board
Thanks Don,
That's a great response, and very supportive... You saved me, and saved me a lot of money!
However,
My vermiculite is quite old, because I had been using for years, my Dysson, until it broke. Recently.
So my verm. Is with shelf primer. But did not get thru rigidizing.
Do you think I can do the rigidizing NOW ?..
Do I have to scrap, or sand the kilnwash before rigidizing?
I shall be grateful for your response
From the very bottom of my heart!
That's a great response, and very supportive... You saved me, and saved me a lot of money!
However,
My vermiculite is quite old, because I had been using for years, my Dysson, until it broke. Recently.
So my verm. Is with shelf primer. But did not get thru rigidizing.
Do you think I can do the rigidizing NOW ?..
Do I have to scrap, or sand the kilnwash before rigidizing?
I shall be grateful for your response
From the very bottom of my heart!
Last edited by Havi on Thu Jan 22, 2015 11:35 am, edited 2 times in total.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Vermiuculite board
I can't imagine that rigidizing would help vermiculite board, or that kilnwash would hurt it. Relying on paper is certainly a reasonable approach. Don mentions powdering his board to fill in the holes. This makes sense to me. Plain alumina hydrate is more durable than kilnwash that is half EPK (kaolin clay).
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Vermiuculite board
Thanks, Bert
HaVi
HaVi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Vermiuculite board
Some more questions -
Can I dry the rigidized vermiculite in the kiln, or does it have to air dry??
Can I apply kiln wash on the wet rigidized shelf and have them dry together?
Can I dry the kilnwashed vermi. inside the kiln?
At what temp. should any of this be done, if this is possible? For how long????
Can I rigidize both sides of the verm. and kiln dry them?
Thanks!!!!!
HaVi
Can I dry the rigidized vermiculite in the kiln, or does it have to air dry??
Can I apply kiln wash on the wet rigidized shelf and have them dry together?
Can I dry the kilnwashed vermi. inside the kiln?
At what temp. should any of this be done, if this is possible? For how long????
Can I rigidize both sides of the verm. and kiln dry them?
Thanks!!!!!
HaVi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Vermiuculite board
Havi wrote:Some more questions -
Can I dry the rigidized vermiculite in the kiln, or does it have to air dry??
Bert has already said there is no necessity (or in my opinion, any advantage) to rigidise.
Can I apply kiln wash on the wet rigidized shelf and have them dry together?
Not a good idea
Can I dry the kilnwashed vermi. inside the kiln?
Yes
At what temp. should any of this be done, if this is possible? For how long????
Drying kiln was can be done at 99C, depending on how much moisture you put in it. A mirror over a port hole will fog up if there is still steam coming out
Can I rigidize both sides of the verm. and kiln dry them?
Yes if you must do it at all
Thanks!!!!!
HaVi
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: Vermiuculite board
Thanks, Richard
- - -
To be on the safe side.
I want the shelf to survive as long as possible.
Meanwhile I have already rigidized both sides
Thanks anyway,
HaVi
- - -
To be on the safe side.
I want the shelf to survive as long as possible.
Meanwhile I have already rigidized both sides
Thanks anyway,
HaVi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com