I want to experiment with making color bars (I think that's the term), but I have a kiln that heats from the sides. Since the glass will be surrounded by dams, is it possible to make these bars? Will the dams allow enough heat to get to the glass?
Disclaimer: I'm new to glass fusing so forgive me if it's a silly question.
Molly
Making color bars in a ceramic kiln
Moderator: Tony Smith
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Making color bars in a ceramic kiln
Not a problem. I do it all the time.