Page 1 of 1
Bullseye Alchemy & silver stain
Posted: Fri Feb 27, 2015 11:04 am
by Don Burt
I got some of Bullseye's two 'Alchemy' clear glasses and tried some silver stain on it. THese are light applications of airbrushed silver stain from different manufacturers. The BE1015 looks like it more reactive than the tin side of float glass. Neither glass seems as reactive to my stains as BE1009.

Re: Bullseye Alchemy & silver stain
Posted: Mon Mar 02, 2015 3:50 pm
by psh
Don,
Thank you for posting your silver stain test strips. I recently purchased a small amount of Reusche silver stain and am still researching how to use it and what type of results are possible - big learning curve needed on my end! I appreciate you pushing me forward!
All the best,
Patty
Re: Bullseye Alchemy & silver stain
Posted: Mon Mar 02, 2015 8:07 pm
by Don Burt
Thanks Patty. Ken Leap's Silver Stain book is a valuable source of info. Its a small book, and kind of expensive, but it was worth it to me.
http://www.blurb.com/b/1693981-silver-stain
Re: Bullseye Alchemy & silver stain
Posted: Tue Mar 03, 2015 9:41 pm
by psh
Thanks Don!