Page 1 of 1

Pot melt COE 96

Posted: Mon Mar 09, 2015 8:57 am
by Outrigger42
The manufacturer of my kiln says it will not withstand 1700. How do I do a pot melt at lower temperature. I am using one of Patty Grays 5 hole molds.

Re: Pot melt COE 96

Posted: Mon Mar 09, 2015 12:53 pm
by Judd
I've done pot melts at 1650. Gil Reynolds does his low-temp- wire pours at 1465.

Re: Pot melt COE 96

Posted: Thu Mar 12, 2015 8:21 pm
by Sharol
You can get the glass to flow at lower temperature you'll just need to hold it at top temp longer. Depending on your kiln, 1650 or 1675 will work. You don't mention how much glass you will have in the pot, but take a peak after about a 45 minute hold at top temperature to see how things are going. Add more time as you need to.

Re: Pot melt COE 96

Posted: Tue Mar 17, 2015 4:17 pm
by Janet McFadyen
1500 f works just fine for S96