MR97 problems HELP
Posted: Sun Jun 28, 2015 10:04 am
Ok - so I just bought a new kiln and I'm still learning the ins and outs. I also bought a new texture mold, the 12" Tree of Life. I sprayed it with MR97. I prefused the 1st one with silver iridized and black with a full fuse - the irid side down on the black, then put it on the mold and fused using Laurie Spray's schedule. It blew a bubble - my fault. The second one I didn't prefuse, put the irid side down on the mold, then black, then fused - same schedule but with a longer bubble squeeze. No bubble, BUT the MR97 stuck to the glass. My top temp was 1470 for 10 minutes. I scrubbed it off, but now there is a haze especially in the leaves that I can't scrub out. Can anyone tell me what I did wrong? How can I get rid of the haze. I tried soaking in vinegar, but that did nothing. I can post a picture (I think) if anyone needs it. Thanks to everyone. I've been gone for about two months as my husband was hospitalized, and he finally had a heart transplant this past week.
What a miracle!
Patty
Patty