help, need answer asap

Posted: Thu Feb 19, 2004 7:17 pm
by bkrgrl@aol.com
Am getting ready to fire some jewelry pieces and the kiln wash is not dry in the bottom of the kiln-it is fairly new and shop owner told me to coat bottom with wash-now I can't get it dry. tried running it up to 100-it srill is damp-I plan to put pieces on shelf, it is dry-dare I put the stuff in and fire-will it dry on the way up if I go slow? thanks waiting with the lid up! bkrgrl

Posted: Thu Feb 19, 2004 7:20 pm
by charlie
you mean the bottom of the kiln isn't dry, but the shelves are? sure go ahead.

the wash on the bottom is to protect against glass spills. if it spills off your shelf on this firing, it'll be dry long before the spill.

Posted: Thu Feb 19, 2004 7:32 pm
by bkrgrl@aol.com
Thanks Charlie, I'll go start now! where are you in az.? My son lives Scottsdale. Gayle